Floor Standing Versatile Automatic Abrasive Cutter AICUT-300 Brief Introduction: The iqualitrol AICUT-300 series are floor standing automatic cutters with high performance. This is a versatile cutting machine designed for sectioning an extremely wide range of materials, such as metals, fasteners, ... Read More
|
|
|
Automatic Precision Saw AutoCUT 200B Support Automatic and Manual Cutting Brief Introduction: The iqualitrol AutoCUT 200B is a tabletop precision sectioning saw with both automatic and manual cutting capabilities. This is a versatile cutting machine designed for sectioning circuit boards and a ... Read More
|
|
|
Menu Structure Touch Screen Digital Rockwell Hardness Tester CHRS-150M Brief Introduction: The iqualitrol CHRS-150M touch screen Rockwell hardness tester features a large screen display and a menu-based structure. It can test all Rockwell scales, including Rockwell and plastic Rockwell. It can ... Read More
|
|
|
Metal Fatigue Failure and Characteristics Fatigue failure refers to the phenomenon that metal materials fail due to cumulative damage after a certain number of cycles under the action of variable loads. Fatigue failure has a certain degree of contingency and randomness, and the probability of ... Read More
|
|
|
Fully Split Coating Thickness Gauge iqualitrol MC-3001 with Separated Measuring Probes Technical Specifications: Measurement Range by Probes Type N0.5: 0-0.5㎜ F0.5: 0-0.5㎜ F1.2: 0-1.25㎜ N1.2: 0-1.25㎜ F3: 0-3㎜ F5: 0-5㎜ F10: 0-10㎜ Measurement Mode Simplified Mode, Monitoring Mode, Statistics Mode, ... Read More
|
|
|
Select Temperature Range of Climate Chamber At present, the temperature range of environment test chambers is generally -40℃~150℃. Some test equipment can reach a low temperature of -70℃ and a high temperature of 180℃. For -40℃~150℃, unless there is a special need, such as the installation location ... Read More
|
|
|
What is Metal Low-Cycle Fatigue Fracture? Parts that experience low-cycle fatigue fracture are subjected to forces that are close to or exceed the yield strength of the material, with a relatively low loading rate, usually measured in minutes, hours, or even longer periods. One characteristic of low... Read More
|
|
|
Mechanical Fatigue Fracture Fatigue fractures account for the highest proportion of fracture failures. To determine whether a component's fracture is due to fatigue, it is not difficult to judge based on the macroscopic morphology of the fracture surface and the stress conditions. Combining this ... Read More
|
|
|
What is Brinell Hardness Test? The Brinell hardness test method consists of indenting the test material with a 10 mm diameter hardened carbide ball subjected to a load of 3000 kg. For softer materials the load can be reduced to 1500 kg or 500 kg to avoid excessive indentation. The full load is ... Read More
|
|
|
Auto Turret Digital Brinell Hardness Tester CHBS-3000MZ with Touch Screen Controller Brief Introduction: CHBS-3000MZ Automatic Turret Digital Display Touch Screen Brinell Hardness Tester. The instrument adopts electric loading and unloading of the test force, with feedback provided by a pressure ... Read More
|